Effect of Zener-Hollomon parameter on deformation microstructure in Fe-3%Si alloy |
| |
Authors: | Fenghui AN Yuhui SHA Fang ZHANG Liang ZUO Key Laboratory for Anisotropy Texture of Materials Northeastern University Shenyang China |
| |
Affiliation: | Fenghui AN,Yuhui SHA*,Fang ZHANG and Liang ZUO Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education),Northeastern University,Shenyang 110819,China |
| |
Abstract: | Hot deformation of Fe-3%Si alloy within the temperature range of 1073-1473 K and strain rate range of 0.01-5 s-1 was carried out by compression test.Optical microscopy (OM),electron backscattered diffraction (EBSD) and transmission electron microscopy (TEM) were used to characterize the deformation microstructure on various scales.Dynamic recovery is the dominant softening mechanism under all experimental conditions.A dynamic recovery region and partial dynamic recrystallization region can be distinguished ... |
| |
Keywords: | Fe-3%Si Hot deformation Microstructure Zener-Hollomon parameter |