首页 | 本学科首页   官方微博 | 高级检索  
     

8090 Al-Li合金激光焊及焊后的组织与性能
引用本文:王蕾,石崇刚. 8090 Al-Li合金激光焊及焊后的组织与性能[J]. 中国激光, 1999, 26(10): 951-954
作者姓名:王蕾  石崇刚
作者单位:南京航空航天大学材料科学与工程系,南京,210016
摘    要:研究了8090Al-Li合金的YAG激光焊,通过金相观察、显微硬度测定以及电子探针微区成分分析,结果表明:在一定的焊接工艺参数下,能得到优良的焊接接头。单面焊能焊厚度≤0.7mm,双面焊能焊厚度≤1.4mm,焊缝为细晶组织,焊缝窄,热影响区小,焊后应即时去应力处理。

关 键 词:Al-Li合金  激光焊  焊接接头
收稿时间:1998-04-24

Welding of Joints of 8090 Al-Li Alloy by Laser Welding and Their Structure and Properties
Wang Lei,Shi Chonggang. Welding of Joints of 8090 Al-Li Alloy by Laser Welding and Their Structure and Properties[J]. Chinese Journal of Lasers, 1999, 26(10): 951-954
Authors:Wang Lei  Shi Chonggang
Abstract:Welded joints of Al-Li alloy welded by YAG laser are investigated through metalloscopy, micro-hardness and electron probe micro-analysis. The results showed that a suitable welded joint can be obtained under proper welding parameters. The thoroughly penetrated thickness does not exceed 0. 7 mm for the single impulse welding and 1. 4 mm for the double impulse welding. The we1d is narrow and has a fine grain structure while the wideness of the heat affected zone is small. Moreover, a stress releasing treatment must be done as soon as possible after welding.
Keywords:Al-Li alloy   laser welding   weld joint
本文献已被 CNKI 万方数据 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号