温差比例控温退火技术在3003H26薄带生产中的应用
引用本文:吴丹. 温差比例控温退火技术在3003H26薄带生产中的应用[J]. 有色金属材料与工程, 2012, 0(3): 122-126
作者姓名:吴丹
作者单位:江阴新仁科技有限公司,江苏江阴214407
摘    要:以3003铝合金铸轧坯料生产H26状态0.20mm厚度板材产品为例,介绍了温差比例控温退火技术在生产实践中的应用。

关 键 词:温差比例  3003铝合金  退火技术  H26状态  应用

Application of Proportional Temperature Difference Control Annealing Technology in 3003H26 Sheet Production
WU Dan. Application of Proportional Temperature Difference Control Annealing Technology in 3003H26 Sheet Production[J]. Nonferrous Metal Materials and Engineering, 2012, 0(3): 122-126
Authors:WU Dan
Affiliation:WU Dan ( Jiangyin Xinren Technology Co., Ltd., Jiangyin 214407, China)
Abstract:Taking the production of 3003H26 sheet with thickness 0.20mm produced out from the semi finished material 3003 east AI alloy rolls as an example, this article presents an introduction of the application of annealing technology featured in controlling temperature difference proportion during the whole process in production practice.
Keywords:temperature difference proportion  3003 A1 alloys  annealing technology  H26condition  application