30CrMnSiNi2A钢疲劳裂纹形成寿命表征与预测
引用本文:黄宏发,阎海,陶春虎. 30CrMnSiNi2A钢疲劳裂纹形成寿命表征与预测[J]. 材料工程, 1997, 0(5)
作者姓名:黄宏发  阎海  陶春虎
作者单位:北京航空材料研究院
摘    要:采用耐久性分析方法 ,由断口金相数据得到参考裂纹扩展时间 (TTCI)的概率分布函数 ,由 TTCI概率分布函数和约束条件得到了通用当量初始缺陷尺寸 (EIFS)的概率分布函数。

关 键 词:参考裂纹形成时间(TTCI)  当量初始缺陷尺寸(EIFS)

Characterizing and Prediction of30 Cr Mn Si Ni2 A Fatigue Crack Initiation Time
Huang Hongfa Yan Hai Tao Chunhu. Characterizing and Prediction of30 Cr Mn Si Ni2 A Fatigue Crack Initiation Time[J]. Journal of Materials Engineering, 1997, 0(5)
Authors:Huang Hongfa Yan Hai Tao Chunhu
Abstract:The a- t data from fracture surface are analysed by an equation of crack growth rate that is often used in durability.Weibull distribution is used to describe the distribution of reference crack initia- tion time.Equivalent initial faults sizes distribution characterizing a group of specimens with the same con- figuration under spectrum loading is finished.From the results,the TTCI distribution probabilities about different stress levels and crack lengths could be obtained.
Keywords:reference crack initiation time ( TTCI) equivalent initial faults size ( EIFS)