基金项目:湖南省自然科学基金(2020JJ4507,2020JJ5456);;湖南省教育厅科学研究重点资助项目(19A413);
摘    要:以过硫酸钠为氧化剂, 在碳酸钠溶液中从低品位铜精矿中提取钼。运用单因素实验法, 探讨了搅拌速度、过硫酸钠和碳酸钠初始浓度、浸出时间、温度和液固比等因素对氧化碱浸提取钼的影响。结果表明,铜精矿氧化碱浸提取钼的优化条件为: 搅拌速度500 r/min, 浸出温度50 ℃, 碳酸钠初始浓度2.5 mol/L, 过硫酸钠初始浓度0.7 mol/L, 液固比10 mL/g, 浸出时间4.0 h, 在此条件下钼浸出率达97.10%。

关 键 词:铜精矿  氧化碱浸    过硫酸钠  氧化剂  
收稿时间:2021-12-27

Extraction of Molybdenum from Low-Grade Copper Concentrate by Persulfate Oxidation and Alkali Leaching
WANG Tie-mo,LIU Zhi-xiong,LI Fei,LI Qin-xiang,LI Guang-ying,LIU Jia-qi,ZHANG Jing-sen,DUAN Xiao-yue.Extraction of Molybdenum from Low-Grade Copper Concentrate by Persulfate Oxidation and Alkali Leaching[J].Mining and Metallurgical Engineering,2022,42(3):104-107.
Authors:WANG Tie-mo  LIU Zhi-xiong  LI Fei  LI Qin-xiang  LI Guang-ying  LIU Jia-qi  ZHANG Jing-sen  DUAN Xiao-yue
Abstract:With sodium persulfate as an oxidant, molybdenum was extracted from a low-grade copper concentrate in sodium carbonate solution. The effects of stirring speed, initial concentration of sodium persulfate and sodium carbonate, leaching time and temperature, as well as liquid-solid ratio on molybdenum extraction rate by oxidative alkaline leaching were investigated by performing single factor experiment. Results show that the leaching rate of molybdenum can reach 97.10%, after molybdenum is extracted from copper concentrate by using oxidative alkaline leaching at 50 ℃ for 4 h, with stirring speed at 500 r/min, initial concentration of sodium carbonate and sodium persulfate at 2.5 mol/L and 0.7 mol/L respectively, liquid-solid ratio at 10 mL/g.
Keywords:copper concentrate  oxidative alkaline leaching  molybdenum  sodium persulfate  oxidant  