脱硫醇尾气管线腐蚀分析与防护
引用本文:晁全水,居建龙. 脱硫醇尾气管线腐蚀分析与防护[J]. 石油化工腐蚀与防护, 2001, 18(2): 28-29
作者姓名:晁全水  居建龙
作者单位:1. 洛阳石油化工总厂炼油厂二联合,河南省,洛阳市,471003
2. 江苏吴县锅检所,江苏省,苏州市,215128
摘    要:针对脱硫醇装置尾气管线的湿硫化氢腐蚀问题,提出了用氮气吹扫管线等有效措施,特别指出选用0Crl7Ni7Mo2不锈钢是最有效的办法,其腐蚀率为0.07mm/a.

关 键 词:脱硫醇装置  尾气管线  硫化氢  腐蚀  缓蚀剂  氮气吹扫'0Clr7N订Mo2不锈钢
修稿时间:2000-10-18

Analysis of Corrosion of Tail Gas Pipeline in Sweetening Unit and Protection
Chao Quanshui,Ju Jianlong. Analysis of Corrosion of Tail Gas Pipeline in Sweetening Unit and Protection[J]. Petrochemical Corrosion and Protection, 2001, 18(2): 28-29
Authors:Chao Quanshui  Ju Jianlong
Abstract:The effective measures such as nitrogen purging, etc, were proposed based upon the hydrogen sulfide corrosion conditions of the tail gas pipeline of sweetening unit. Among these measures, selection of 0Cr17Ni7Mo2 stainless steel was the most cost-effective way to reduce the corrosion. The annual corrosion rate was only 0.07 mm.
Keywords:sweetening unit   tail gas pipeline   hydrogen sulfide   corrosion   corrosion inhibitor   nitrogen purging   0Cr17Ni7Mo2 stainless steel