氢氧化钾/石油焦质量配比对活性炭性能的影响
引用本文:张红波,伍恢和.氢氧化钾/石油焦质量配比对活性炭性能的影响[J].功能材料,1996,27(6):565-568.
作者姓名:张红波  伍恢和
作者单位:湖南大学化学化工系,湖南长岭炼油化工总厂研究院
摘    要:本文以石油焦为原料,采用氢氧化钾化学活化法系统考察了氢氧化钾/焦炭的质量配比(碱/炭,Wb/Wc)对活性炭吸附性能和孔隙性能的影响。结果表明,随着碱/炭比的增加,吸附性能显著提高;比表面积,总孔容积,微孔容积和非微孔容积都增加;孔径分布变窄,平均孔径减少。碱/炭比大于等于3∶1时,所得活性炭试样的比表面积大于3000m2/g。

关 键 词:氢氧化钾  石油焦  活性炭  性能

Effects of the Weight Ratio between Potassium Hydroxide and Petroleum Coke on Properties of Activated Carbon
Zhang Hongbo,Wu Huihe Liu Hongbo.Effects of the Weight Ratio between Potassium Hydroxide and Petroleum Coke on Properties of Activated Carbon[J].Journal of Functional Materials,1996,27(6):565-568.
Authors:Zhang Hongbo  Wu Huihe Liu Hongbo
Abstract:The effects of the weight ratio between potassium hydroxide and petroleum coke (Wb/Wc) on the adsorption properties and pore properties of activated carbon were studied by a direct chemical activation routein which petroleum coke was reacted with excess potassium hydroxide.Results show that with the increase of Wb/Wc,adsorption properties rise remarkably;specific surface areas,volumes of total pore,micropores and non micropores increase;pore size distribution becomes narrow and average pore diameter decreases.When Wb/Wc is greater than or equal to 3 to 1,specific surface areas of activated carbor are greadter than 3000m 2/g.
Keywords:Potassium hydroxide  Petroleum coke  activated Carbon  property