摘    要:对锌冶炼含铟窑渣综合回收新工艺进行优化,考察酸度、液固比、时间、温度等对锌和铟浸出率的影响以及不同酸度下金属铟的走向,得到最优工艺条件。在二段浸出后铟综合回收率为82.8%。

关 键 词:次氧化锌    浸出  优化  回收率
收稿时间:1/2/2012 3:49:26 PM
修稿时间:1/2/2012 3:50:35 PM

Study on Comprehensive Recovery of Low Arsenic Secondary Zinc Oxide Dust
Yi Chao,Lu Xingwu and Ma Aijun.Study on Comprehensive Recovery of Low Arsenic Secondary Zinc Oxide Dust[J].Nonferrous Metals(Extractive Metallurgy),2012(8):7-10.
Authors:Yi Chao  Lu Xingwu and Ma Aijun
Affiliation:Northwest Institute of Mining and Metallurgy,,
Abstract:A new comprehensive recovery process from zinc smelting slag with indium content was optimized. The effects of acidity, ratio of liquid to solid, time, temperature on the leaching rate of zinc and indium were investigated, and whereabouts of metal indium with a variety of acidity were studied. The optimal process conditions were obtained. The results show that the overall recovery of indium is 82.8% after two step leaching.
Keywords:secondary zinc oxide dust  indium  leaching  optimization  recovery rate