首页 | 本学科首页   官方微博 | 高级检索  
     


Influence of H4SiW12O40 loading on hydrocracking activity of non-sulfide Ni-H4SiW12O40/SiO2 catalysts
Authors:Hao Jin  Xiaodan Sun  Weizheng Weng  Huilin Wan
Affiliation:State Key Laboratory for Physical Chemistry of the Solid Surfaces, Engineering Laboratory for Green Chemical Productions of Alcohols, Ethers and Esters, College of Chemistry and Chemical Engineering, Xiamen University, Xiamen 361005, PR China
Abstract:The effect of H4SiW12O40 loading on the catalytic performance of the reduced Ni-H4SiW12O40/SiO2 catalysts for hydrocracking of n-decane with or without the presence of thiophene and pyridine is studied. The catalysts were characterized by BET, XRD, Raman, XPS, H2-TPR, H2-TPD, NH3-TPD and FT-IR of pyridine adsorption. It was found that addition of H4SiW12O40 to the system increases the catalytic activity and the promoting effect is a function of the H4SiW12O40 loading. The best result was obtained on 5%Ni-50%H4SiW12O40/SiO2 catalyst which shows the highest activity for hydrocracking of n-decane and excellent tolerance to the sulfur and nitrogen compounds in the feedstock. The results showed that a suitable amount of H4SiW12O40 loading on the 5%Ni/SiO2 catalyst increases the amount of both hydrogen adsorbed and Brønsted acid and Lewis acid sites on the catalyst. The high catalytic performance of the catalyst can be related to the nature of H4SiW12O40 and the proper balance between metal and acid functions.
Keywords:Hydrocracking   Bifunctional catalyst   Ni   H4SiW12O40   n-Decane
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号