摘    要:通过对芳纶1414纤维助染剂预处理,进行阳离子染料染色实验,探讨染色工艺参数对芳纶1414纤维染色性能的影响。实验表明,染色最佳工艺为染料用量5%(omf),助染剂用量2%,氯化钠用量15g/L,染浴pH为4.5,染色温度110℃,染色保温时间60min;染色后耐皂洗色牢度可达到4~5级。

关 键 词:聚对苯二甲酰对苯二胺纤维  阳离子染料  染色  助染剂

Dyeing properties of para-aramid fiber pretreated with dyeingg-auxiliary
WANG Jian-wei, WANG Hua, TAN Yan-jun. Dyeing properties of para-aramid fiber pretreated with dyeingg-auxiliary[J]. Textile Dyeing and Finishing Journal, 2012, 34(9): 19-22
Authors:WANG Jian-wei   WANG Hua   TAN Yan-jun
Affiliation:(Faculty of Textile and Material, Xi’an Polytechnic University, Xi’an 710048, China)
Abstract:Para-aramid fiber was firstly pretreated with dyeing auxiliary, and then dyed with cationic dye. The dyeing technological parameters were explored and the optimized dyeing technological conditions are as follows: dye concentration 5%(omf), dyeing auxiliary 2%, sodium chloride 15 g/L, pH of dyeing bath is 4.5, dyeing temperature was kept at 110 ℃ for 60 min. The color fastness to washing can reach 4~5 grade.