Abstract: | Three kinds of high-purity A12O3 powders, whose average paticle size is 0. l, 0.3 and 3.0 mp respectively, were used as thestarting power, and their compacts were fired in the radio-frequency plasma generated at a pressure of 80 Pa using N, as the working gas.Experimental results show that the 0. 1 and 0.3 mp powder compacts can be sintered to nearly the theoretical density within 60 s and thissintering is almost finished in the heating period. It is concluded that the mechanism of liquid sintering, the electric charge effect of Al2O3powder, and the effect of tempetrature gradient in the compacts can affect simultaneously on the rapid densification of the compacts inthe plasma sintering. |