摘    要:研究了3种不同含Ti量(0.04%-0.16%Ti)钢奥氏体晶粒粗化温度及热轧后奥体再结晶的行为。在950-1200℃加热,含0.04%Ti钢奥氏体晶粒最小,其晶粒开始粗化温度在1 150℃以上。得出含Ti钢开始再结晶的临界形变率(εc)与原始奥氏体晶粒直径(D0)、轧制温度(T)间定量关系。

关 键 词:奥氏体晶粒  再结晶  临界形变量  轧制温度
收稿时间:1992-06-17

Austenite Grain Coarsening and Recrystallization Parameters of Steel Containing Titanium
Li Xiuqiu, Cui Wenxuan. Austenite Grain Coarsening and Recrystallization Parameters of Steel Containing Titanium[J]. Chinese Journal of Engineering, 1993, 15(1): 82-85. DOI: 10.13374/j.issn1001-053x.1993.01.014
Authors:Li Xiuqiu  Cui Wenxuan
Abstract:The temperature of austenite grain coarsening and recrystallization parameters in steels containing 0.04%-0.16% Ti have been investigated.Experimental results show that after heating at 950-1 200℃,austenite grain size in 0.04% Ti-steel was the finest, and the temperature of grain coarsening was above 1 150℃.The quantitative relationship between the critical reduction for austenite recrystallization εc and initinal austenite grain size Do at rolling temperature T has been obtained
Keywords:austenite grain  recrystallization  critical reduction  rolling temperature