首页 | 本学科首页   官方微博 | 高级检索  
     

顺北油田抗超高温柔性胶粒修井液
引用本文:康红兵,牛骋程,贾虎,高定祥,代昌楼. 顺北油田抗超高温柔性胶粒修井液[J]. 钻井液与完井液, 2021, 38(4): 525-530. DOI: 10.3969/j.issn.1001-5620.2021.04.020
作者姓名:康红兵  牛骋程  贾虎  高定祥  代昌楼
作者单位:1.中国石油化工集团公司碳酸盐岩缝洞型油藏提高采收率重点实验室,乌鲁木齐 830011
基金项目:霍英东青年教师基金(171043);四川省区域创新合作项目(20QYCX0064);四川省杰出青年科技人才项目(2019JDJQ0036)
摘    要:针对顺北高温油气井常规增黏型修井液易降解的难题,基于高分子柔性胶粒分散-降解-提黏-稳黏理论,研发了抗180 ℃ 高温柔性胶粒修井液体系,该修井液动力黏度在20~140 mPa·s范围可调,密度在1.0~1.3 g/cm3可调,实现了固相与无固相加重。明确了修井液在不同温度下的黏度变化规律,高温180 ℃ 高温老化1 d后黏度明显高于传统黄原胶体系,表现出良好的稳黏性能,该修井液对铝合金材料的腐蚀速率不超过2.22 g/(m2·h),并且携砂效果显著。该研究对顺北高温油气井安全高效修井作业具有一定指导意义。 

关 键 词:超高温   柔性胶粒   修井液   稳黏   密度可调   铝合金   腐蚀
收稿时间:2021-02-28

Ultra-High Temperature Workover Fluid with Flexible Rubber Particles Used in Shunbei Oilfield
Affiliation:1.Key Laboratory of Enhanced Oil Recovery in Carbonate Fractured-vuggy Reservoirs, CNPC, Urumqi, Xinjiang 8300112.Research Institute of Petroleum Engineering, SINOPEC Northwest Company of China Petroleum and Chemical Corporation, Urumqi, Xinjiang 8300113.School of Petroluem Engineering, Southwest Petroleum University, Chengdu, Sichuan 610500
Abstract:The conventional viscosified workover fluid used in the high temperature oil and gas wells in Shunbei Oilfield is easy to lose its viscosity. To solve this problem, a new workover fluid containing flexible rubber particles that is able to resist 180 ℃ was developed based on the fact that the viscosity of a flexible high molecular weight rubber particle changes in a pattern of “disperse, degrade, viscosify, and stabilize viscosity”. The dynamic viscosity of this workover fluid can be adjusted between 20 mPa·s and 140 mPa·s. The density of the workover fluid adjusted between 1.0 g/cm3 and 1.3 g/cm3, which means that the workover fluid can be weighted with or without solid weighting agents. The pattern of the viscosity change of the workover fluid at different temperatures was studied. After aging for 1 day at 180 ℃, the viscosity of the workover fluid was apparently higher than that of a conventional xanthan gum workover fluid, indicating that the new workover fluid had the ability of stabilizing its viscosity. The rate of corrosion of this workover fluid to aluminum alloy is less than 2.22 g/(m2·h). The workover fluid also had very good sand carrying capacity. This study has certain guiding significance for the safe and efficient workover operations of high-temperature oil and gas wells in Shunbei. 
Keywords:
本文献已被 CNKI 等数据库收录!
点击此处可从《钻井液与完井液》浏览原始摘要信息
点击此处可从《钻井液与完井液》下载全文