Recovery of copper values from bio-heap leaching of low grade Malanjkhand chalcopyrite ore
Authors:Lala Behari Sukla  Kailash Chandra Nathsarma  Joystna Rani Mahanta  Sradhanjali Singh  Snehasis Behera  Karanam Srinivas Rao  Tondepu Subbaiah  Barada Kanta Mishra
Affiliation:(1) Chemistry Department, Faculty of Science, Beni-Suef University, Beni-Suef, Egypt;(2) Nuclear Material Authority, P.O. Box 530, El Maddi, Cairo, Egypt;
Abstract:M/S Hindustan Copper Limited (HCL), India generates large amounts of lean sulfide ores of copper. The current production of lean copper ores in India is 0.55 million tons with ∼0.3% average copper content. Heap-bioleaching of the lean copper ores in 15 and 30 ton scales was undertaken at IMMT, Bhubaneswar. The leaching study showed 0.09% dissolution of copper from the ore body per day. The leach liquor was processed through solvent extraction and electrowinning. Extraction of copper from the actual leach liquor was carried out with 1.5% LIX 622N in kerosene with zero co-extraction of iron. The copper-free raffinate was fed back to the leaching unit. Stripping of copper from the loaded organic was carried out with 180 kg/m3 H2SO4. The copper pregnant electrolyte was passed through a carbon column to make it free from entrained organic and was fed to the electrowinning unit. The increase in current efficiency was due to the increase in the concentration of electrolyte. The energy consumption was 1.7 kWh/kg at a flow rate of 4.5 L/h. Smooth and bright sheets of copper of 99.99% purity were obtained.
Keywords:
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号