Hot-working characteristics of C and V HSLA steels
Authors:HJ McQueen  O Overdal  A Cingara  H Gjestland
Abstract:The 0.045% V HSLA and the C steel were deformed in torsion over the range 850–1150°C and 0.1–30 s?1. Flow stress, temperature and strain rate were related by the combination of the Arrhenius function with either the exponential or sinh functions. Based on peak stress from the sinh equation and a linear peak strain dependence, an equation is proposed for calculating flow curves. The constants in the exponential law were evaluated at strain intervals of 0.05 up to ε = 0.5, so that flow curves and mean pass stresses could be estimated for any rolling condition. Calculated and measured roll separating forces were compared for a nine-pass schedule. Ferrite grain size increased linearly with rising T at constant ε and ε. In multistage, isothermal tests after pass strains of 0.3, the fractional softening for delay times of 1, 10 and 30 s were determined. In mill simulations of nine passes with T declining from 1270 to 750°C, the pass flow curves and the finishing grain sizes were determined. The behaviours of the steels are contrasted and also compared with those of other HSLA steels.
Keywords:HSLA steels  hot working  flow curves
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号