首页 | 本学科首页   官方微博 | 高级检索  
     

Electrochemical properties and structure of MlNi_(5-x)Sn_x system
作者单位:Qin Lin,Dajian Zhu,and Shuang ZhaoMetallurgy School,University of Science and Technology Beijing,Beijing 100083,China
摘    要:The electrochemical properties and structure of M1Ni5-xSnx(x=0-0.5) hydrogen storage alloys were investigated by pressure-composition isotherms, electrochemical measurements, X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS) and atomic parameters. With a small amount of tin substitution, the cycle life increases by 52% (0.5C) and 42% (1.0C), but maximum discharge capacity decreases only by 3.0% and 3.5%, respectively. The cycle life is obviously improved by the low volume expansion and the formed SnO2 surface layers upon electrochemical cycling. The substitution of Ni by Sn leads to an increase of the unit cell volume and charge-discharge cycle life and decrease of the plateau pressure, hysteresis and the hydrogen storage capacity. The standard enthalpy of hydride formation decreases with increasing tin substitution. The main factor that influences the standard enthalpy of the hydriding reaction is the number of the outer orbit electrons and not the atomic size factor.


Electrochemical properties and structure of MlNi5-xSnx system
Authors:Qin Lin  Dajian Zhu  Shuang Zhao
Abstract:The electrochemical properties and structure of MlNi5-xSnx(x=0-0.5) hydrogen storage alloys were investigated by pressure-composition isotherms, electrochemical measurements, X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS) and atomic parameters. With a small amount of tin substitution, the cycle life increases by 52% (0.5C) and 42% (1.0C), but maximum discharge capacity decreases only by 3.0% and 3.5%, respectively. The cycle life is obviously improved by the low volume expansion and the formed SnO2 surface layers upon electrochemical cycling. The substitution of Ni by Sn leads to an increase of the unit cell volume and charge-discharge cycle life and decrease of the plateau pressure, hysteresis and the hydrogen storage capacity. The standard enthalpy of hydride formation decreases with increasing tin substitution. The main factor that influences the standard enthalpy of the hydriding reaction is the number of the outer orbit electrons and not the atomic size factor.
Keywords:hydrogen storage alloy  MlNi5-xSnx  electrochemical properties  structure