减少无缝钢管退火氧化措施探讨
引用本文:张学成,蒋素芳,魏玉芝,李桂林,翟国营,魏鹏. 减少无缝钢管退火氧化措施探讨[J]. 河南冶金, 2001, 0(1): 8-10
作者姓名:张学成  蒋素芳  魏玉芝  李桂林  翟国营  魏鹏
作者单位:安阳钢铁集团有限公司
摘    要:分析了无缝钢管退火中的氧化因素,结合生产实际,提出了减少无缝钢管氧化的措施.实践证明,采取的措施是有效的.

关 键 词:无缝钢管  退火  氧化  影响因素  措施
修稿时间:2000-10-20

DISCUSSION ON METHODS TO REDUCE OXIDATION IN ANNEALING OF SEAMLESS STEEL TUBE
Zhang Xuecheng Jiang Sufang Wei YuzhiLi Guilin Zhai Guoying Wei Peng. DISCUSSION ON METHODS TO REDUCE OXIDATION IN ANNEALING OF SEAMLESS STEEL TUBE[J]. Henan Metallurgy, 2001, 0(1): 8-10
Authors:Zhang Xuecheng Jiang Sufang Wei YuzhiLi Guilin Zhai Guoying Wei Peng
Affiliation:Anyang Iron & Steel Group Co. Ltd.
Abstract:Oxidation factors in annealing of seamless steel tube are analyzed, combining with production practice,some methods have been put forward to decrease oxidation of seamless steel tube. The operational results shows that the control methods taken are effective.
Keywords:seamless steel tube annealing oxidation effectors method