Abstract: | Vanadyl phthalocyanine (VOPc) crystal thin films were prepared on poly(ethylene terephthalate) (PET) film. The VOPc film prepared on PET substrate at 120 °C had Phase II. The third harmonic (TH) intensity of the VOPc film was measured by the marker fringe method. The third optical susceptibility (χ(3)) estimated from TH intensity is 3.5 × 10?9 esu. The transition from Phase I to Phase II of the VOPc film was enhanced with corona charging. © 2002 Wiley Periodicals, Inc. Electr Eng Jpn, 140(2): 36–43, 2002; Published online in Wiley InterScience ( www.interscience.wiley.com ). DOI 10.1002/eej.10022 |