Nitroxide‐terminated poly(styrene‐co‐diethyl fumarates) and derived block copolymers
Authors:J Lokaj  P Holler  J Kovr&#x;ov
Affiliation:J. Lokaj,P. Holler,J. Kovár̆ová
Abstract:Copolymerization of styrene (S) and diethyl fumarate (DEF) at 125°C in the presence of 2,2,6,6‐ tetramethylpiperidin‐1‐yloxyl radical (TEMPO) and initiated with a thermal initiator, 2,2′‐azobisisobutyronitrile (AIBN), was studied. The molar fraction of DEF in the feed, FDEF, varied within 0.1–0.9. An azeotropic composition, (FDEF)A = 0.38, was found for the copolymerization under study. At FDEF = 0.1–0.4, a quasi‐living process was observed, transforming to a retarded conventional radical copolymerization at a higher content of DEF in the initial mixtures. The obtained TEMPO‐terminated S‐DEF copolymers were used to initiate polymerization of styrene. Poly(styrene‐ co‐diethyl fumarate)‐block‐polystyrene copolymers were prepared with molecular weight distributions depending on the amount of inactive polymer chains in macroinitiators, as indicated by size‐exclusion chromatography. A limited miscibility of the blocks in the synthesized block copolymers was revealed by using differential scanning calorimetry. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 84: 2432–2439, 2002
Keywords:styrene‐diethyl fumarate comonomers  nitroxide‐terminated copolymers  quasi‐living copolymerization  block copolymers
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号