首页 | 本学科首页   官方微博 | 高级检索  
     


Enhancing adhesive joints between commercial rubber (SBS) and polyurethane by low-pressure plasma surface modification
Affiliation:1. Chair of Aroma and Smell Research, Emil Fischer Center, Department of Chemistry and Pharmacy, Friedrich-Alexander-University Erlangen-Nürnberg, Henkestraße 9, 91054, Erlangen, Germany;2. Department Sensory Analytics, Fraunhofer Institute for Process Engineering and Packaging IVV, Giggenhauser Straße 35, 85354, Freising, Germany;1. School of Engineering and Technology, Walailak University, Nakhon Si Thammarat, 80160, Thailand;2. Center of Excellence on Wood and Biomaterials, Walailak University, Nakhon Si Thammarat, 80160, Thailand;3. Center of Excellence on Petrochemical and Materials Technology, Bangkok, 10330, Thailand;4. School of Science, Walailak University, Nakhon Si Thammarat, 80160, Thailand;5. Department of Physics, Rajarajeswari College of Engineering, Bangalore, India
Abstract:The paper presents research on the two-stage process of low-pressure plasma surface modification of a commercial SBS rubber, improving its adhesion to both the polyurethane adhesive in an organic solvent (PU) and the aqueous polyurethane adhesive dispersion (ADPU). The plasma surface modification process was carried out in a flow reactor with parallel plate electrodes, in which plasma was generated by an RF glow discharge (13.56 MHz). In the first stage of the process, the Ar or O2 plasma was used, and then, as the second stage of the modification process, the treatment was performed in H2O plasma. The adhesive properties of the plasma-modified SBS rubber surface were determined using the 180o-peel strength test (PS). These results were correlated with surface properties investigated using contact angle (CA) measurements, FTIR-ATR spectroscopy, XPS spectroscopy and scanning electron microscopy (SEM). The observed improvement in wettability of the plasma modified surface was attributed to the formation of hydroxyl groups, which was confirmed by spectroscopic methods (FTiR-ATR and XPS). The results of the 180o-peel strength test showed, in turn, a clear relationship between the capacity of adhesive bonding and the amount of oxygen groups (mainly the hydroxyl groups) as well as the surface roughness, determined by SEM microscopy. It was also found that the effects of the plasma surface modification of the SBS rubber were stable for at least 72 h. The results of this work prove that cleaning and etching of the commercial SBS rubber surface in the first stage of its plasma treatment, followed by chemical modification in the second stage, lead to very strong adhesive joints.
Keywords:SBS rubber  Adhesive bonding  Plasma treatment  X-ray photoelectron spectroscopy
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号