Abstract: | The interfacial adhesion of blend of isotactic polypropylene/poly(vinyl methylether) (i‐PP/PVME) has been improved by the addition of poly(propylene‐g‐acrylic acid) (PP‐g‐AA) as a compatibilizing agent. The phase morphologies of the blends are investigated by optical microscopy (OM) and lateral force microscopy (LFM). The i‐PP/PVME (80/20) blend with no addition of PP‐g‐AA from extrusion process shows a coarse morphology with the dispersed domain size as large as several micrometers; After the addition of 2.5% PP‐g‐AA in the blends, the dispersed PVME domain size decreases greatly. The addition of 5% PP‐g‐AA results in a homogeneous morphology. The blending of PP‐g‐AA with PVME reduces the crystallization temperature of PP‐g‐AA, which is different from that of blending i‐PP with PVME. The increase of the interfacial adhesion is attributed to the specific intermolecular interaction between the acrylic acid group of PP‐g‐AA and the ether group of PVME. The specific interaction is studied by Fourier transform infrared spectroscopy. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 4098–4103, 2006 |