  • Abstract:Spark plasma sintering technique was used for the consolidation of nanostructured titanium carbide synthesized by mechanical alloying in order to avoid any important grain growth of the compact materials. The TiC phase was obtained after about 2 h of mechanical alloying. Towards the end of the milling process (20 h), the nanocrystalline powders reached a critical size value of less than 5 nm. Some physical and mechanical properties of the consolidated carbide were reported as a function of the starting grain size powders obtained after different mechanical alloying durations. The crystalline grain size of the bulk samples was found to be increased to a maximum of 120 nm and 91 nm for carbides mechanically alloyed for 2 h and 20 h respectively. The Vickers hardness showed to be improved to about 2700 Hv for a maximum density of 95.1% of the bulk material.
    Keywords:Nanostructured TiC carbide  Mechanical alloying  Spark plasma sintering technique  Density consolidation  Hardness
    本文献已被 ScienceDirect 等数据库收录!
    设为首页 | 免责声明 | 关于勤云 | 加入收藏

    Copyright©北京勤云科技发展有限公司  京ICP备09084417号