首页 | 本学科首页   官方微博 | 高级检索  
     

方坯连铸机漏钢原因分析及改进措施
引用本文:叶途明,肖卫军,何金平,王金平,赵中福.方坯连铸机漏钢原因分析及改进措施[J].炼钢,2009,25(2).
作者姓名:叶途明  肖卫军  何金平  王金平  赵中福
作者单位:武汉钢铁(集团)公司第一炼钢厂,湖北,武汉,430083
摘    要:统计了武钢一炼钢厂方坯连铸机2006年的漏钢情况,分析了粘结漏钢和角部纵裂漏钢的特点及机理,并找出了产生粘结漏钢和角部纵裂漏钢的主要原因是保护渣的性能、结晶器的精度、钢水的过热度、拉速及浸入式水口的对中等.采取了相应的措施后铸机的漏钢率有了明显的降低.

关 键 词:方坯连铸  粘结  角部纵裂  漏钢

Analysis on breakout of bloom continuous caster and countermeasures
YE Tu-ming,XIAO Wei-jun,HE Jin-ping,WANG Jin-ping,ZHAO Zhong-fu.Analysis on breakout of bloom continuous caster and countermeasures[J].Steelmaking,2009,25(2).
Authors:YE Tu-ming  XIAO Wei-jun  HE Jin-ping  WANG Jin-ping  ZHAO Zhong-fu
Affiliation:No.1 Steelmaking Plant;WISCO;Wuhan 430083;China
Abstract:The statistics of breakout of the bloom continuous caster in No.1 steelmaking plant of WISCO in 2006 have been made and the main characteristics and mechanism of sticking breakout and longitudinal corner crack induced breakout analyzed.The main causes to the above mentioned breakouts are found to be such a few factors as the performance of mold powder,accuracy of mold,extent of hot metal overheat,casting speed,and alignment of the submerged entry nozzle with the mold and etc,and thereupon certain countermea...
Keywords:bloom continuous casting  sticking  longitudinal corner crack  breakout  