有孤立热节的小铸件缩孔解决方法
引用本文:吕存昌. 有孤立热节的小铸件缩孔解决方法[J]. 特种铸造及有色合金, 2002, 0(2): 33-34
作者姓名:吕存昌
作者单位:广东南海智恒精密铸造厂
摘    要:对有孤立热节的小铸件产生缩孔的原因进行了分析,通过提高型壳温度和浇注温度可减少和消除缩孔的产生,针对不同铸件采用不用的组树方案,以及增设铸造圆角均可有效地减少缩孔。

关 键 词:孤立热节 小铸件 精密铸造 缩孔 浇注温度
文章编号:1001-2449(2002)02-0033-02
修稿时间:2001-09-20

The Ways for Elimination of Shrinkage Hole in Light Casting with Isolated Hot Spot
Lv Cunchang. The Ways for Elimination of Shrinkage Hole in Light Casting with Isolated Hot Spot[J]. Special Casting & Nonferrous Alloys, 2002, 0(2): 33-34
Authors:Lv Cunchang
Abstract:The reason for shrinkage hole in light casting with isolated hot spot was analyzed. The shrinkage hole can be reduced and eliminated through increasing molding shell temperature and pouring temperature. The shrinkage hole can be decreased effectively through adopting different assembly tree schemes for different castings and adding round corner in casting also.
Keywords:Investment Casting   Shrinkage Hole   Pouring Temperature  