基于纳米二氧化硅改性下SAP内养护混凝土的基本性能研究* |
| |
引用本文: | 姜佩弦,刘荣桂,张灵灵.基于纳米二氧化硅改性下SAP内养护混凝土的基本性能研究*[J].水泥工程,2024,37(1):69-78. |
| |
作者姓名: | 姜佩弦 刘荣桂 张灵灵 |
| |
作者单位: | 南通理工学院 |
| |
摘 要: | 研究纳米二氧化硅(NS)改性SAP内养护混凝土的物理力学性能以及抗氯离子渗透性能,提出该混凝土的配合比设计。复掺0.08%SAP和1.5%NS能提高混凝土抗折强度;复掺0.08%SAP和1.0%NS能提高其抗压强度;复掺0.24%SAP和1.5%NS氯离子抗渗透性能最佳;复掺0.24%SAP和0.5%NS能显著减小干燥收缩率。
|
关 键 词: | 纳米二氧化硅 SAP内养护混凝土 标准养护 抗压强度 凝结时间 |
Research on the basic properties of SAP internal curing concrete based on nano silica modification |
| |
Abstract: | The physical and mechanical properties and chloride ion penetration resistance of nano-silica (NS) modified SAP internal curing concrete are studied, and the mix design of this concrete is put forward. The bending strength of concrete can be improved by adding 0.08% SAP and 1.5% NS.The compressive strength of concrete can be improved by adding 0.08% SAP and 1.0% NS. The permeability resistance of chloride ion is the best by adding 0.24% SAP and 1.5% NS. Adding 0.24% SAP and 0.5% NS can significantly reduce the drying shrinkage. |
| |
Keywords: | nano silica modification SAP internal curing concrete compressive strength setting time |
|