冶炼不锈钢30 t EBT电弧炉炉衬寿命的提高
引用本文:岑永权,沙国平,潘路影,吴国庆. 冶炼不锈钢30 t EBT电弧炉炉衬寿命的提高[J]. 特殊钢, 2003, 24(1): 47-48
作者姓名:岑永权  沙国平  潘路影  吴国庆
作者单位:1. 上海应用技术学院,上海200233
2. 上海三钢公司
摘    要:上海三钢公司特钢厂改进不锈钢初炼电弧炉操作工艺、造渣制度和采用炉渣发泡技术后 ,使初炼炉炉衬寿命从 3 0炉提高到 60炉以上 ,保证 2台EBT电弧炉与 1台AOD相匹配。

关 键 词:不锈钢  偏心炉底电弧炉  AOD  炉衬寿命  泡沫渣
修稿时间:2002-07-12

Increasing of Lining Service Life of a 30 t EBT Arc Furnace for Stainless Steel Melting
Cen Yongquan. Increasing of Lining Service Life of a 30 t EBT Arc Furnace for Stainless Steel Melting[J]. Special Steel, 2003, 24(1): 47-48
Authors:Cen Yongquan
Abstract:The lining service life of a 30 t arc furnace for stainless steel melting at Special Steel Works, Shanghai No3 Steel Co has been increased from 30 heats to more than 60 heats by improving the operation skill,the slag|making procedure and the applied slag foaming technique to ensure two set of EBT arc furnace matching an AOD unit.
Keywords:Stainless Steel   EBT Arc Furnace   AOD   Furnace Lining Service Life   Foaming Slag
本文献已被 CNKI 万方数据 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号