首页 | 本学科首页   官方微博 | 高级检索  
     

梅山铁矿铁精矿降硅选矿工艺试验
引用本文:勾金玲,徐望华. 梅山铁矿铁精矿降硅选矿工艺试验[J]. 现代矿业, 2013, 29(7): 26
作者姓名:勾金玲  徐望华
作者单位:宝钢集团(南京)梅山矿业公司选矿厂
摘    要:为进一步满足冶炼对铁精矿质量的要求,梅山铁矿选矿厂需降低铁精矿中SiO2的含量。为此,对生产出的强磁精矿进行了正浮选和细筛-再磨强磁选2种工艺流程的降硅试验研究。试验结果表明:2种工艺都能有效降低总精矿中的SiO2含量至4%以下,虽回收率有所损失,但最终精矿的碱比明显提高,矿石的自熔性变好,建议对这2种工艺进行试验室扩大连续试验和工业试验,以为现场技术改造提供参考依据。

关 键 词:铁精矿  降硅  正浮选  细筛&mdash  再磨强磁选工艺  

Beneficiation Tests on Reduce Silicon of Iron Concentrate in Meishan Iron Plant
Gou Jinling , Xu Wanghua. Beneficiation Tests on Reduce Silicon of Iron Concentrate in Meishan Iron Plant[J]. Modern Mining, 2013, 29(7): 26
Authors:Gou Jinling    Xu Wanghua
Affiliation:Concentrator of BaoSteel Group (Shanghai) Meishan Mining Co. Ltd.
Abstract:Reduce the content of SiO2 in iron ore concentrate become a necessity for Meishan iron ore, in order to well meet the smelting requirements of iron ore quality. Study was conducted with positive flotation and fine sieve-regrinding and strong magnetic process separately. The results showed that: both of the two process could ruduce the content of SiO2 to 4% in total concentrate, though recovery rate was lower, but the alkali ratio significantly increased, and the self-fluxing quality become better. Laboratory and industrial tests was suggested to continue, in order to provide reference basis for on-site process.
Keywords:Iron concentrate  Reduce of silicon  Positive flotation  Fine sieve-regrinding and high intensity magnetic process  
本文献已被 万方数据 等数据库收录!
点击此处可从《现代矿业》浏览原始摘要信息
点击此处可从《现代矿业》下载全文