摘    要:为了生产高磁感取向硅钢板用板坯,钢中添加Bi:0.0005%~0.05%,加入时,在中间包的外侧的钢水池中形成上围堰,并且用被覆了铁的圆桶,桶内装入Bi或Bi的合金加入到钢水中,钢水流量除以喷嘴内面积求出浸渍喷嘴内的钢水流量密度Q(≥0.9t/(m^2·s^-1)),为了使结晶内液面形成旋流,采用电磁搅拌,其推力F要满足关系式(3.000≤F≤10.000Pa·m^-1)。

关 键 词:高磁感取向硅钢  板坯  Bi

CASTING CAST SLABS OF HIGH MAGNETIC FUX DENSITY GRAIN ORIENTED SILICON STEEL SHEET
Lu Fengxi.CASTING CAST SLABS OF HIGH MAGNETIC FUX DENSITY GRAIN ORIENTED SILICON STEEL SHEET[J].Metallurgical Information Review,2009(2):39-42.
Authors:Lu Fengxi
Affiliation:Lu Fengxi (The WISCO Wuhan 430080 )
Abstract:To stably produce cast slabs of ultra high Magnetic Fux Density Grain Oriented Silicon Steel Sheet, the content of Bi in the steel is controlled to 0.000 5% to 0.05%, a region divided by providing an upper weir is formed in a molten steel pool on the outlet side of a tundish, and, as an iron-coated wire filled with Bi or a Bi alloy is fed into the region, the flow rate density Q of the molten steel in an immersion nozzle obtained by dividing the flow rate of the molten steel by the inner area of the nozzle, and the thrust F of electromagnetic stirring for forming a rotating flow in the vicinity of the molten steel surface satisfy the relational inequalities, provide means for advantageously solving unstableness which is a problem when a Bi-containing phase is utilized as an inhibitor forming.