摘    要:根据原矿中白钨矿呈细粒嵌布的特点,采用全浮工艺流程,以碳酸钠为调整剂,水玻璃为脉石矿物的抑制剂,ZL为捕收剂浮选回收白钨矿。对含WO31.43%的原矿获得了含WO3为32.34%的白钨中间精矿,钨粗选回收率95.32%;通过常温精选与加温精选比较试验,对钨中间精矿确定采用加温精选,获得了含WO3为66.16%,回收率91.78%的精矿。

关 键 词:白钨矿  细粒嵌布  全浮选  加温精选

Experimental Research on Beneficiation of a Yunnan Scheelite Mine
Lin Rixiao,Zhang Faming,Zeng Qingjun,Chen Zhijie,Zhang Xianhua.Experimental Research on Beneficiation of a Yunnan Scheelite Mine[J].Metal Mine,2011,40(3):74-77.
Authors:Lin Rixiao  Zhang Faming  Zeng Qingjun  Chen Zhijie  Zhang Xianhua
Affiliation:Guangzhou Research Institute of Nonferrous Metals;
Abstract:According to the characteristics of fine-grained disseminated scheelite in run-of-mine, the scheelite was concentrated by adopting the full flotation process with sodium carbonate as regulator agent, sodium silicate as inhibitor for the gangue minerals, and ZL Pharmacy as collector. 32.34% of the coarse scheelite concentrate (WO3) with tungsten recovery of 95.32% was obtained from the raw ores with grade of 1.43%. Through the comparison tests between concentration at normal temperature and heating temperature, it was determined to concentrate the rough tungsten by heating, by which the high-quality scheelite with tungsten (WO3) of 66.16% and tungsten concentrate recovery of 91.78% was obtained.
Keywords:Scheelite  Fine dissemination  Full flotation  Heating concentration
本文献已被 万方数据 等数据库收录!
点击此处可从《金属矿山》浏览原始摘要信息
点击此处可从《金属矿山》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号