磷酸盐反应釜用C-276+16MnR复合板的腐蚀原因分析
引用本文:万建春,郑世平.磷酸盐反应釜用C-276+16MnR复合板的腐蚀原因分析[J].压力容器,2006,23(11):34-35,54.
作者姓名:万建春  郑世平
作者单位:南京斯迈柯特种金属装备有限公司,江苏,南京,211102
摘    要:通过化学分析、金相分析和ASTMG28腐蚀试验等方法,对磷酸盐反应釜用C-276+16MnR复合板的腐蚀原因进行了分析。结果表明,腐蚀是由于不恰当的热处理造成材料敏化而产生的。

关 键 词:C-276  16MnR复合板  腐蚀  热处理
文章编号:1001-4837(2006)11-0034-02
收稿时间:2006-11-07
修稿时间:2006-11-07

Corrosion Analysis of C-276+16MnR Clad Steel Plate Used in Reactor of Phosphate
WAN Jian-chun,ZHENG Shi-ping.Corrosion Analysis of C-276+16MnR Clad Steel Plate Used in Reactor of Phosphate[J].Pressure Vessel Technology,2006,23(11):34-35,54.
Authors:WAN Jian-chun  ZHENG Shi-ping
Affiliation:Nanjing Special Metal Equipment Co., Ltd., Nanjing 211102,China
Abstract:By means of chemical and metallographic phase analysis and ASTM G28 corrosion test to analyze the corrosion of C-276 16MnR clad steel plate used in the Reactor of Phosphate.The results indicated that the corrosion was caused by sensitization,which was resulted from improper heat treatment.
Keywords:C-276 16MnR clad steel plate  corrosion  heat treatment