Service tests of chrome-spinel-periclase refractories |
| |
Authors: | V. P. Semyannikov Yu. I. Savchenko V. A. Perepelitsyn L. I. Koval'chuk I. D. Kashcheev V. I. Ignat'ev |
| |
Affiliation: | (1) All-Union Refractory Institute, USSR;(2) S. M. Kirov Ural Polytechnic Institute, USSR;(3) Izhorskii Plant Production Union, USSR |
| |
Abstract: | Conclusions In chemical composition the experimental chrome-spinel-periclase refractories are characterized by a high degree of purity. The total content of impurity oxides of silicon, calcium, and iron does not exceed 2%. The parts possess increased density, porosity, and slag resistance but a lower heat resistance than the imported refractories with a silica content of 0.5%.Comparative tests of the experimental chrome-spinel-periclase parts (area of about 0.5 m2) and the imported refractories with a silica content of 0.5% in the slag belt of an ASEA-SKF installation ladle showed similar lives of them. For a final experimental test it would be desirable to produce a larger experimental production lot of the chrome-spinel-periclase refractories and to test them in the slag zone of ASEA-SKF ladles.Translated from Ogneupory, No. 1, pp. 44–47, January, 1985. |
| |
Keywords: | |
本文献已被 SpringerLink 等数据库收录! |
|