Modification of polyamide 6 with hycar ATBN |
| |
Authors: | Vladimír Marouek Petr Svoboda Jaroslav Krliek |
| |
Affiliation: | Vladimír Maroušek,Petr Svoboda,Jaroslav Králišek |
| |
Abstract: | The preparation of block copolymers from 6-caprolactam and a liquid amine terminated butadiene-acrylonitrile copolymer Hycar ATBN 1300X21 having higher notched impact strength than ordinary poly(6-caprolactam) was studied. In the polymerization of 6-caprolactam initiated by an adduct of phosphoric acid with 6-caprolactam the influence of initiator concentration (0– 50 mol-%) and Hycar ATBN 1300X21 concentration (0–5 wt.-%) in the polymerization charge, of polymerization time (4 – 72 h) and of temperature (200–280°C) on the 6-caprolactam conversion and on the properties of the copolymers formed were followed. Notched impact strength of the block copolymers prepared under optimized conditions was as high as 13.5 kJ·m?2. |
| |