摘    要:某发电公司1900吨锅炉高温再热器(TP347H)进口段于168试运行期间爆破,爆口张开很大成喇叭状,并从喇叭口中部断成二截。笔者通过宏观检查、化学成份分析、金相检测等项目试验分析,得出:某发电公司高温再热器爆管原因为长时加短时超温爆管,为异物堵塞造成。并介绍了长时超温即蠕变断裂机理——应力集中断裂机理。

关 键 词:超临界机组  锅炉高温再热器  长时超温

Analysis on Tube Burst in Boiler High-temperature Reheater of Supercritical Unit
Abstract:The inducer of a 1900t boiler high-temperature reheater(TP347H) burst in supercritical unit of a power plant during 168 pre-operation,the site of burst was trumpet-shaped and the trumpet broke into two pieces form center.Some conclusions are achieved by some experiments such as: macro inspection,chemical constitution analysis and metallographic detection,etc.They are as follows: long-term and short-term over-temperature and foreign body obstruction are the reasons of bursting.And the mechanism of creep fracture and stress concentration fracture is long-term overtemperature.
Keywords:supercritical unit  boiler high-temperature reheater  long-term overtemperature