首页 | 本学科首页   官方微博 | 高级检索  
     

西北某难选铁矿石选矿试验
引用本文:苗梁,李国栋,姜永智,陈杜娟. 西北某难选铁矿石选矿试验[J]. 金属矿山, 2013, 43(3): 73-76
作者姓名:苗梁  李国栋  姜永智  陈杜娟
作者单位:1.西北矿冶研究院;2.北京科技大学土木与环境工程学院
摘    要:西北某难选铁矿石中主要铁矿物为磁铁矿和镜铁矿,其中磁铁矿与镜铁矿、镜铁矿与石英嵌布关系密切。对该矿石进行了磨选工艺技术条件研究,结果表明,采用磨矿-1粗1精弱磁选-强磁粗选-强磁粗精矿再磨-强磁精选流程处理,可以获得铁品位为66.39%、回收率为40.94%的弱磁精矿和铁品位为63.41%、回收率为37.27%的强磁精矿,综合精矿铁品位为64.95%、回收率为78.21%。

关 键 词:磁铁矿  镜铁矿  弱磁选  强磁选

Experimental Research on Beneficiation of a Refractory Iron Ore at Northwest of China
Miao Liang , Li Guodong , Jiang Yongzhi , Chen Dujuan. Experimental Research on Beneficiation of a Refractory Iron Ore at Northwest of China[J]. Metal Mine, 2013, 43(3): 73-76
Authors:Miao Liang    Li Guodong    Jiang Yongzhi    Chen Dujuan
Affiliation:1.Northwest Research Institute of Mining &Metallurgy;2. School of Civil and Environmental Engineering,University of Science and Technology Beijing;
Abstract:There are mainly magnetite and specularite in a refractory iron ore at northwest of China, among which magnetite and specularite, specularite and quartz have a closely disseminated relationship. The technical conditioning tests for grinding and concentration of the ore are carried out. The results showed that low intensity magnetic concentrate with Fe grade of 66.39% and recovery of 40.94% and high intensiy magnetic concentrate with Fe grade of 63.41% and Fe recovery of 37.27% were obtained by the process of grinding-low intensity magnetic separation with one roughing and one cleaning-rough high intensity magnetic separation-regrinding of rough concentrate-cleaning concentration with high intensity magnetic separation. Total Fe concentrate is grading at 64.95% with the recovery of 78.21%.
Keywords:Magnetite  Specularite  Low intensity magnetic separation  High intensity magnetic separation
本文献已被 万方数据 等数据库收录!
点击此处可从《金属矿山》浏览原始摘要信息
点击此处可从《金属矿山》下载全文