HgCdTe/Si materials for long wavelength infrared detectors
Authors:S M Johnson  A A Buell  M F Vilela  J M Peterson  J B Varesi  M D Newton  G M Venzor  R E Bornfreund  W A Radford  E P G Smith  J P Rosbeck  T J De Lyon  J E Jensen  V Nathan
Affiliation:(1) Raytheon Vision Systems, 93117 Goleta, CA;(2) HRL Laboratories LLC, 90265 Malibu, CA;(3) Air Force Research Laboratory, AFRL/VSSS, Kirtland AFB, 87117, NM
Abstract:The heteroepitaxial growth of HgCdTe on large-area Si substrates is an enabling technology leading to the production of low-cost, large-format infrared focal plane arrays (FPAs). This approach will allow HgCdTe FPA technology to be scaled beyond the limitations of bulk CdZnTe substrates. We have already achieved excellent mid-wavelength infrared (MWIR) and short wavelength infrared (SWIR) detector and FPA results using HgCdTe grown on 4-in. Si substrates using molecular beam epitaxy (MBE), and this work was focused on extending these results into the long wavelength infrared (LWIR) spectral regime. A series of nine p-on-n LWIR HgCdTe double-layer heterojunction (DLHJ) detector structures were grown on 4-in. Si substrates. The HgCdTe composition uniformity was very good over the entire 4-in. wafer with a typical maximum nonuniformity of 2.2% at the very edge of the wafer; run-to-run composition reproducibility, realized with real-time feedback control using spectroscopic ellipsometry, was also very good. Both secondary ion mass spectrometry (SIMS) and Hall-effect measurements showed well-behaved doping and majority carrier properties, respectively. Preliminary detector results were promising for this initial work and good broad-band spectral response was demonstrated; 61% quantum efficiency was measured, which is very good compared to a maximum allowed value of 70% for a non-antireflection-coated Si surface. The R0A products for HgCdTe/Si detectors in the 9.6-μm and 12-μm cutoff range were at least one order of magnitude below typical results for detectors fabricated on bulk CdZnTe substrates. This lower performance was attributed to an elevated dislocation density, which is in the mid-106 cm−2 range. The dislocation density in HgCdTe/Si needs to be reduced to <106 cm−2 to make high-performance LWIR detectors, and multiple approaches are being tried across the infrared community to achieve this result because the technological payoff is significant.
Keywords:HgCdTe  heteroepitaxy  infrared detectors  molecular beam epitaxy (MBE)  HgCdTe/Si  long wavelength infrared (LWIR)
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号