PBT—BCF的研制
引用本文:王延春.PBT—BCF的研制[J].合成纤维工业,1992,15(3):6-8.
作者姓名:王延春
摘    要:利用PP-BCF设备研制生产PBT-BCF,要求PBT切片η]为0.9dL/g,干燥后含水≤2.5‰;PBT-BCF生产中纺丝温度控制在低于PET纺丝温度10—15℃;可用PP色母粒原液着色生产有色丝;纺丝油剂可用PET长丝油剂;并对产品的性能和用途作了简要介绍。

关 键 词:聚对苯二甲酸丁二酯  纤维  膨体变形长丝  原液着色

THE TECHNOLOGY FOR PRODUCING PBT BULK CONTINUOUS FILAMENT (BCF)
Abstract:The technology for producing PBT-BCF by using PP-BCF spinning machine was studied. The viscosity η] of raw material PBT is 0.9 and water content 2.5‰ after drying. The spinning temperature is controlled 10-15℃ lower than that of PET. PBT -BCF can be dope-dyed with master batch for PP fiber. The spinning finish for PET filament yarn is applicable to PBT-BCF. The property and application of raw mate- rial and products are introduced in this paper.
Keywords:polybutylene terephthalate (PBT)  bulk continuous filament (BCF)  dope dyeing