摘    要:通过改进调质工艺,使用8%-10%的无机水基淬火液,改进淬火冷却工艺参数,解决了42Cr Mo4钢齿圈淬火开裂的问题。

关 键 词:42Cr  Mo4  齿圈  调质处理  淬火裂纹

Quenching and Tempering for 42 CrMo4 Steel Forged Gear Ring
Wang Songlin,Ren Xiufeng,Zhang Yongqing,Liu Shoufeng,Yin Wei,Wang Cong.Quenching and Tempering for 42 CrMo4 Steel Forged Gear Ring[J].Heavy Casting and Forging,2014(6):21-26.
Authors:Wang Songlin  Ren Xiufeng  Zhang Yongqing  Liu Shoufeng  Yin Wei  Wang Cong
Affiliation:Wang Songlin, Ren Xiufeng, Zhang Yongqing, Liu Shoufeng, Yin Wei, Wang Cong
Abstract:By improving the tempering and quenching process,8%-10% of inorganic water-based quenching liquid is used to improve the quench cooling process parameters and solve the crack problem during 42 Cr Mo4 steel gear ring quenching.
Keywords:42CrMo4  gear ring  quenching and tempering  quenched crack