High‐resolution thermogravimetry of poly(2,6‐dimethyl‐1,4‐phenylene oxide)
Authors:Xin‐Gui Li
Abstract:The thermal degradation and kinetics of poly(2,6‐dimethylphenylene oxide) (PPO) were studied by high‐resolution thermogravimetry. The thermogravimetry measurements were conducted at an initial heating rate of 50°C min−1, resolution 4.0, and sensitivity 1.0 in both nitrogen and air from room temperature to 900°C. A two‐step degradation process was clearly revealed in air at the temperatures of 430°C and 521°C. The thermal degradation temperatures and kinetic parameters of the PPO appear to be higher in air than in nitrogen, indicative of a higher thermostability in air. The temperature, activation energy, order, and frequency factor of the thermal degradation of the PPO in nitrogen are 419°C, 100–120 kJ mol−1, 0.5, and 13–17 min−1, respectively. © 1999 John Wiley & Sons, Inc. J Appl Polym Sci 71: 1887–1892, 1999
Keywords:poly(2  6‐dimethylphenylene oxide)  high‐resolution thermogravimetry  thermal degradation  degradation kinetics  thermostability
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号