10 micrometer-scale SPM local oxidation lithography
Authors:Toyofuku Takashi  Nishimura Shinya  Miyashita Kazuya  Shirakashi Jun-ichi
Affiliation:Department of Electrical and Electronic Engineering, Tokyo University of Agriculture and Technology, Koganei, Tokyo 184-8588, Japan.
Abstract:10 micrometer-scale scanning probe microscopy (SPM) local oxidation lithography was performed on Si. In order to realize large-scale oxidation, an SPM tip with a contact length of 15 microm was prepared by focused-ion-beam (FIB) etching. The oxidation was carried out in contact mode operation with the contact force ranging from 0.1 to 2.1 microN. The applied bias voltage was 50 V, and scanning speed was varied from 10 to 200 microm/s. The scan length was 15 microm for one cycle. The influence of contact force on the large-scale oxidation was investigated. At high contact force, the Si oxide with good size uniformity was obtained even with high scanning speed. The SPM tip with larger contact length may increase the spatial dimensions of the water meniscus between the SPM tip and sample surface, resulting in the larger dimensions of the fabricated oxide. Furthermore, the throughput of large-scale oxidation reached about 10(3) microm2/s by controlling the scanning speed and contact force of the SPM tip. It is suggested that SPM local oxidation can be upscaled by using a SPM tip with large contact length.
Keywords:
本文献已被 PubMed 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号