首页 | 本学科首页   官方微博 | 高级检索  
     


Partial pore blockage and polymer chain rigidification phenomena in PEO/ZIF-8 mixed matrix membranes synthesized by in situ polymerization
Authors:Xiaoli Ding  Xu Li  Hongyong Zhao  Ran Wang  Runqing Zhao  Hong Li  Yuzhong Zhang
Affiliation:1. State Key Laboratory of Separation Membranes and Membrane Processes/National Center for International Joint Research on Separation Membranes, Tianjin Polytechnic University, Tianjin 300387, China;2. Tianjin Key Laboratory of Hollow Fiber Membrane Materials and Processes, Tianjin Polytechnic University, Tianjin 300387, China;3. Institute of Separation Material and Process Control, School of Material Science and Engineering, Tianjin Polytechnic University, Tianjin 300387, China;4. School of Environmental and Chemical Engineering, Tianjin Polytechnic University, Tianjin 300387, China
Abstract:Nanostructured zeolitic imidazolate frameworks (ZIF-8) was incorporated into the mixture of poly (ethylene glycol) methyl ether acrylate (PEGMEA) and pentaerythritol triacrylate (PETA) to synthesize mixed matrix membranes (MMMs) by in situ polymerization for CO2/CH4 separation.The solvent-free polymerization between PEGMEA and PETA was induced by UV light with 1-hydroxylcyclohexyl phenyl ketone as initiator.The chemical structural characterization was performed by Fourier transform infrared spectroscopy.The morphology was characterized by scanning electron microscope.The average chain-to-chain distance of the polymer chains in MMMs was investigated by X-ray diffraction.The thermal property was evaluated by differential scanning calorimetry.The CH4 and CO2 gas transport properties of MMMs are reported.The relationship between gas permeation-separation performances or physical properties and ZIF-8 loading is also discussed.However,the permeation-separation performance was not improved in Robeson upper bound plot compared with original polymer membrane as predicted.The significant partial pore blockage and polymer rigidification effect around the ZIFs confirmed by the increase in glass temperature and the decrease in the d-sparing,were mainly responsible for the failure in performance improvement,which offset the high diffusion induced by porous ZIF-8.
Keywords:Mixed matrix membrane  Partial pore blockage  Polymer chain rigidification  2
本文献已被 CNKI 万方数据 ScienceDirect 等数据库收录!
点击此处可从《中国化学工程学报》浏览原始摘要信息
点击此处可从《中国化学工程学报》下载全文