The corrosion behaviour of Fe-15Mn-7Si-9Cr-5Ni shape memory alloy |
| |
Authors: | Bikas C. Maji C.M. Das R.K. Ray |
| |
Affiliation: | a Materials Science Division, Bhabha Atomic Research Centre, Mumbai 400 085, India b Materials Processing Division, Bhabha Atomic Research Centre, Mumbai 400 085, India c Department of Materials and Metallurgical Engineering, Indian Institute of Technology, Kanpur 208 016, India |
| |
Abstract: | The corrosion behaviour of Fe-15Mn-7Si-9Cr-5Ni (mass%) shape memory alloy at 25 °C in 0.5 M H2SO4 and 3.5% NaCl solutions has been studied using potentiodynamic polarization and electrochemical impedance techniques. Three different microstructures viz., single-phase γ, γ-δ and γ-Fe5Ni3Si2, were produced by heat-treating the alloy in different equilibrium phase fields. The corrosion behaviour in 0.5 M H2SO4 solution is almost same for all three microstructures, barring a slight difference in the passivation range. Although, the passivation current in 0.5 M H2SO4, is in the same range as that of SS 304, the critical current required for onset of passivation is almost three orders higher and the passivation range is much shorter. In 3.5% NaCl solution the corrosion behaviour of all three microstructures of the Fe-15Mn-7Si-9Cr-5Ni shape memory alloy was that of general dissolution without passivity or localized attack (pitting). The best corrosion resistance in both H2SO4 and NaCl solutions is shown by the single-phase γ microstructure. |
| |
Keywords: | Shape memory alloy Polarization Acid corrosion Pitting corrosion |
本文献已被 ScienceDirect 等数据库收录! |
|