摘    要:钙塑瓦楞纸板是将普通瓦楞纸板的芯纸替换为钙塑材料而成,该材料除普通瓦楞纸板的优点外,还具有强度高、防潮等性能。通过实验方法,对3层钙塑瓦楞复合纸板平压强度、边压强度和戳穿强度进行了测试分析,同时将钙塑瓦楞复合纸板与普通5层瓦楞纸板性能进行了对比。结果表明,3层钙塑瓦楞复合纸板的边压强度为0.650 kN,平压强度为1.274 kN,戳穿强度为7.5 J;5层瓦楞纸板的边压强度为0.378 kN,平压强度为0.437 kN,戳穿强度为6.75 J。为该新材料的推广使用提供了依据。

关 键 词:钙塑瓦楞  复合纸板  平压强度
收稿时间:2013-04-03
修稿时间:2013-06-10

Experimental Study on Properties of Calcium Plastic Composite Corrugated Board
FENG Jun and GAO De. Experimental Study on Properties of Calcium Plastic Composite Corrugated Board[J]. Packaging Engineering, 2013, 34(11): 43-45,92
Authors:FENG Jun and GAO De
Affiliation:1.Taiyuan University of Science and Technology,Taiyuan 030024,China;2.Ningbo Institute of Technology,Zhejiang University,Ningbo 315100,China)
Abstract:Calcium plastic corrugated board is made through substitution of calcium plastic material for ordinary corrugated cardboard, which not only has the advantages of ordinary corrugated cardboard, but also has the advantages of high strength and moisture-proof performance. Flat compression strength, edge crush strength and puncture strength of 3 layer calcium plastic corrugated board were tested and compared with the performance pf ordinary 5 layer corrugated board. The result showed that the flat compression strength, edge crush strength and puncture strength of 3 layer calcium plastic corrugated board is 1. 274 kN, 0. 650 kN, and 6. 75 J respectively; the flat compression strength, edge crush strength and puncture strength of 5 layer corrugated cardboard is 0. 437 kN, 0. 378 kN, and 6. 75 J respectively. The purpose was to provide basis for promotion of the new material application.
Keywords:calcium plastic corrugated board   composite board   flat compression strength