太钢4#高炉大修停炉实践
引用本文:王志军. 太钢4#高炉大修停炉实践[J]. 山西冶金, 2001, 0(2): 14-16
作者姓名:王志军
作者单位:太原钢铁(集团)有限公司炼铁厂,030003
摘    要:太钢4#高炉在大修停炉前保持了长期稳定顺行,停炉过程中采用了大风量、炉项打水等技术措施。实线证明效果良好。

关 键 词:高炉 大修 停炉 大风量 炉顶打水 维修
修稿时间:2001-02-10

The Operation of NO,4B. F. Blowing-off for Relining at TISCO.
Steel Making of TISCO. Wang Zhi jun. The Operation of NO,4B. F. Blowing-off for Relining at TISCO.[J]. Shanxi Metallurgy, 2001, 0(2): 14-16
Authors:Steel Making of TISCO. Wang Zhi jun
Affiliation:Steel Making of TISCO. Wang Zhi jun
Abstract:The operation of NO. 4 blast furnace at TISCO. remainedstable for a long time before its relining in 2000. A series of measures were adopted during the blowing-off. Such as large blast volume, cooling water flow through the top and so on. It shows that these are good points.
Keywords:blast furnace   relining   operation