干膜用聚酯薄膜产生疵点的原因
引用本文:滕岩. 干膜用聚酯薄膜产生疵点的原因[J]. 聚酯工业, 2011, 24(5): 44-45. DOI: 10.3969/j.issn.1008-8261.2011.05.013
作者姓名:滕岩
作者单位:富维薄膜(山东)有限公司,山东潍坊,261061
摘    要:详细介绍并分析了干膜用聚酯薄膜疵点的分类和产生原因。大疵点形成的原因为煳料造成的内部杂质和外来杂质造成的表面杂质,小疵点形成的原因为添加剂粒子团聚造成的内部原因和辊筒烙印造成的表面原因。

关 键 词:聚酯薄膜  干膜  疵点

Defect causes of dry lamination film used PET film
TENG Yan. Defect causes of dry lamination film used PET film[J]. Polyester Industry, 2011, 24(5): 44-45. DOI: 10.3969/j.issn.1008-8261.2011.05.013
Authors:TENG Yan
Affiliation:TENG Yan(Fuwei Film(Shandong)Co.Ltd.,Weifang 261061,China)
Abstract:The classification and causes of defect of dry lamination film used PET film are introduced and analysed in detail.The causes of the big defects are the internal impurity caused by the burnt material and the surface impurity caused by the foreign impurity.The causes of the small defects are the internal reasons caused by the additive particle agglomeration and the surface reasons caused by the roller imprinting.
Keywords:PET film  dry lamination film  defect  