670t/h煤粉锅炉受热面管泄漏综合治理
引用本文:丁厚东,石天佐.670t/h煤粉锅炉受热面管泄漏综合治理[J].发电设备,2006,20(4):240-242,245.
作者姓名:丁厚东  石天佐
作者单位:胜利发电厂,山东,东营,257087;胜利发电厂,山东,东营,257087
摘    要:大型煤粉锅炉受热面管泄漏是影响发电厂安全运行的主要原因之一。分析了胜利发电厂670 t/h超高压煤粉锅炉管泄漏原因,提出了治理措施,从而有效地解决了管子泄漏问题。

关 键 词:能源与动力工程  锅炉  管子泄漏  螺旋肋片管  T91钢  防磨材料
文章编号:1671-086X(2006)04-0240-03
收稿时间:2005-12-29
修稿时间:2005-12-29

Comprehensive Attendance of Tube Leakage of a 670 t/h Coal Fired Boiler's Heat-Delivery Surface
DING Hou-dong,SHI Tian-zuo.Comprehensive Attendance of Tube Leakage of a 670 t/h Coal Fired Boiler's Heat-Delivery Surface[J].Power Equipment,2006,20(4):240-242,245.
Authors:DING Hou-dong  SHI Tian-zuo
Affiliation:Shengli Power Plant, Dongying 257087, China
Abstract:Leakage failure of heat-delivery surface tubes of large coal-fired boilers is one of the main factors affecting safe operation of power plants. The cause of tube leakage occurring to a 670 t/h super-pressure coal-fired boiler is being analyzed, accompanied by some comprehensive countermeasures, which have effectively solved the leakage problem.
Keywords:energy and power engineering  boiler  tube leakage  spirally finned tube  steel T91  erosion resistant material