Fatigue and fracture resistance of minimally invasive ceramic and resin composite veneers with different designs bonded adhesively to severely eroded teeth
Authors:Anita Schwendimann
Affiliation:Clinic for Fixed and Removable Prosthodontics and Dental Materials Science, Center for Dental and Oral Medicine, Dental Materials Unit, University of Zurich, Zurich, Switzerland
Abstract:This study evaluated the load bearing capacity of minimal invasive restoration alternatives on severely worn teeth after cyclic loading. Sound human maxillary incisors (N?=?72, n?=?9 per group) were randomly divided into nine experimental groups to receive one of the following restoration types: Group 1: Intact tooth, Group 2: Direct resin composite, Group 3: Lingual: Indirect resin composite, Labial: Ceramic veneer with lingual overlap, Group 4: Lingual: Indirect resin composite with lingual overlap, Labial: Ceramic, Group 5: Lingual: Direct composite, Labial: Ceramic, Group 6: Lingual: Feldspathic Ceramic, Labial: Feldspathic ceramic, Group 7: Lithium disilicate crown, Group 8: Metal-ceramic crown. Teeth were prepared simulating erosion/wear conditions. Specimens were subjected to cyclic loading (1,200,000 cycles, 5–55?°C) and then loaded to failure from the lingual surface at 105° inclination (1?mm/min). Data (Newton) were analyzed using one-way ANOVA, Tukey`s tests and Weibull moduli were calculated (α?=?0.05). Significant differences were observed between the groups for the initial (p?=?0.006) and maximum fracture load (p?=?0.002). Group 3 (55?±?36) presented significantly lower initial fracture load compared to other groups (79?±?35–134?±?36) (p?<?0.05). When maximum fracture load is considered, control group (1) (602?±?355) and from restored groups 2 (449?±?144) and 4 (495?±?291) showed significantly higher results (p?<?0.05). Weibull modulus for the maximum fracture load was the highest for Group 2 (m?=?3.47) among all groups (m?=?1.61–4.18). Groups 2, 3, 6 presented the highest incidence of repairable failures. Based on the results, severely worn teeth could be restored with lingual direct resin composite and labial veneering with indirect resin with overlap.
Keywords:Erosion  laminates  minimal invasive  static loading  veneers  wear
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号