摘    要:通过静态顶空与气相色谱-质谱联用的方法,探讨了不同温度(80 ℃和130 ℃)和不同硫化温度(130,140,150 ℃)对两种天然橡胶(SVR 3 L和SPR 10#)中挥发性有机化合物(VOCs)的影响。结果表明,130 ℃下,两种天然橡胶中的主要VOCs均能挥发并被检出,SVR 3 L中的VOCs主要是乙醇和乙酸;SPR 10#中除乙醇和乙酸外,主要为醛类物质。硫化温度对两种天然橡胶中VOCs总量的影响不大,说明硫化过程中的高温高压条件可使天然橡胶中的VOCs挥发,硫化胶中的VOCs主要来源于硫化促进剂的热分解产物。

关 键 词:天然橡胶  挥发性有机化合物  挥发  静态顶空  气相色谱-质谱联用

Release of volatile organic compounds from natural rubber at different temperatures
CHEN Xin,ZHANG Bo-yu,WANG Dan-ling,DU Zhen-xia,WU You-ping. Release of volatile organic compounds from natural rubber at different temperatures[J]. China Synthetic Rubber Industry, 2022, 0(1): 17-22. DOI: 10.19908/j.cnki.ISSN1000-1255.2022.01.0017
Authors:CHEN Xin  ZHANG Bo-yu  WANG Dan-ling  DU Zhen-xia  WU You-ping
Affiliation:1.a.Key Laboratory of Beijing City on Preparation and Processing of Novel Polymer Materials, b.College of Science/Beijing Key Laboratory of Environmentally Harmful Chemical Analysis, Beijing University of Chemical Technology, Beijing 100029, China; 2.Zhongce Rubber Group Co Ltd, Hangzhou 310014, China
Abstract:The effects of different temperatures (80 ℃ and 130 ℃) and different vulcanization temperatures (130 ℃, 140 ℃, and 150 ℃) on volatile organic compounds (VOCs) of two natural rubbers (SVR 3 L and SPR 10#) were investigated by static headspace coupled with gas chromatography-mass spectrometry. The results showed that VOCs in the two natural rubbers could be volatilized and detected at 130 ℃, and the VOCs in SVR 3 L were mainly ethanol and acetic acid, while the VOCs in SPR 10# were mainly aldehydes except for ethanol and acetic acid. Different vulcanization temperatures had little effect on total volatile organic compounds in the two natural rubbers, indicating that the high temperature and high pressure conditions in the vulcanization process could cause the volatilization or reaction of VOCs, and the VOCs of vulcanization rubber mainly came from the thermal decomposition products of vulcanization accelerators.
Keywords:natural rubber  volatile organic compounds  volatilization  static headspace  gas chromatography-mass spectrometry
本文献已被 维普 等数据库收录!
点击此处可从《合成橡胶工业》浏览原始摘要信息
点击此处可从《合成橡胶工业》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号