首页 | 本学科首页   官方微博 | 高级检索  
     

AOD炉的高效化冶炼模型
引用本文:艾立翔,汪红兵,徐安军,田乃媛,贺东风.AOD炉的高效化冶炼模型[J].钢铁,2012,47(2):22-25.
作者姓名:艾立翔  汪红兵  徐安军  田乃媛  贺东风
作者单位:1. 北京科技大学冶金与生态工程学院, 北京 100083 2. 北京科技大学高效钢铁冶金国家重点实验室, 北京 100083 3. 北京科技大学计算机与通信工程学院, 北京 100083
基金项目:"十一五"国家科技支撑计划资助项目
摘    要: 以往的AOD炉高效化冶炼研究往往通过提高供氧强度,优化转炉的炉容比,提高终点命中率等技术缩短冶炼周期,需要充分利用现有的设备,优化炉料结构和供氧制度,对生产工艺参数进行优化,充分利用这些物理热和化学热,实现AOD炉的高效化冶炼。开发了AOD炉高效化冶炼模型,在AOD炉物料平衡和能量平衡的基础上,结合AOD炉冶炼的工艺特征,建立AOD炉耗氧量和冶炼周期模型,分析了AOD炉冶炼周期随着铁水比和废钢比的变化趋势,得出冶炼周期最短时的炉料结构。结果表明:电炉不锈钢母液加铁水冶炼时,冶炼周期随着铁水比的增加而增加。电炉不锈钢母液加废钢冶炼时,冶炼周期随着废钢比的增加而增加。铁水加废钢冶炼时,冶炼周期随着废钢比的增加而延长。以硅铁为发热剂比以碳粉为发热剂冶炼周期短。

关 键 词:不锈钢  AOD炉  冶炼周期  
收稿时间:2011-05-12

Efficient Smelting Model of AOD Furnace Steelmaking
AI Li-xiang,WANG Hong-bing,XU An-jun,TIAN Nai-yuan,HE Dong-feng.Efficient Smelting Model of AOD Furnace Steelmaking[J].Iron & Steel,2012,47(2):22-25.
Authors:AI Li-xiang  WANG Hong-bing  XU An-jun  TIAN Nai-yuan  HE Dong-feng
Affiliation:1. School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China 2. State Key Laboratory of Advanced Metallurgy, University of Science and Technology Beijing, Beijing 100083, China 3. School of Computer and Communication Engineering, University of Science and Technology Beijing, Beijing 100083, China
Abstract:The research on traditional AOD efficient smelting was focused on enhancement of oxygen supply,optimization of improving volume ratio,increasing end hitting rate.Current device should be made full of,and AOD charging structure and oxygen supply should be optimized.Process parameters of AOD should be optimized.Physical heat and chemical heat should be rational used,and efficient smelting of AOD should be realized.Based on mass balance model and energy balance model,the model of AOD efficient smelting was proposed considering process features of AOD steelmaking.The change of tap to tap time with hot metal ratio and scrap steel ratio was simulated.The charging structure was got when tap to tap time was the shortest.The results indicate that the tap to tap time increases with molten iron ratio increasing in AOD steelmaking process with EAF stainless molten iron and BF molten iron.The tap to tap time increases with scrap steel ratio increasing in AOD steelmaking process with EAF stainless molten iron and scrap steel.The tap to tap time increases with scrap steel ratio increasing in AOD steelmaking process with BF molten iron and scrap steel.The tap to tap time with ferrosilicon heating agent is shorter than the time with carbon powder heating agent.
Keywords:stainless steel  AOD  tap to tap time
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《钢铁》浏览原始摘要信息
点击此处可从《钢铁》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号