首页 | 本学科首页   官方微博 | 高级检索  
     


Phase separation studies in RIM polyurethanes catalyst and hard segment crystallinity effects
Authors:R.E. Camargo  C.W. Macosko  M. Tirrell  S.T. Wellinghoff
Affiliation:Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, Minnesota 55455, USA
Abstract:Polyurethanes were prepared from pure 4,4′-diphenylmethane diisocyanate (MDI), 1,4-butane diol (BDO) or 1,2-ethane diol (EDO) and α,ω-hydroxyl poly(propylene oxide) (PPO) by reaction injection moulding (RIM). Hard segment (MDI + BDO or EDO) level was 45–50 wt%. The PPO had about 20% ethylene oxide copolymerized in at the chain ends to provide 80% primary OH end groups. Mn was varied from 2000 to 4000. Dibutyl tin dilaurate catalyst and mould temperature were varied. Dynamic mechanical, wide-angle X-ray, differential scanning calorimeter, molecular weight and tensile elongation measurements were made on the RIM polyurethanes. At low reaction rates (low catalyst or temperature) highly crystalline, well phase separated but low molecular weight polymers were produced. At high catalyst or temperature levels more poorly phase separated but high molecular weight, tough polymers resulted. Higher Mn PPO gave better phase separation and EDO gave higher melting temperatures. Preventing hard segment crystallinity by substituting asymmetric MDI or glycols resulted in phase compatibility.
Keywords:polyurethane  reaction injection moulding  polymerization rate  molecular weight  phase separation  crystalline hard segments
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏