钢结构焊缝超声波探伤缺陷当量孔径的计算
引用本文:杨晓东,周鹏,杨芳,尚建丽,王杨俊. 钢结构焊缝超声波探伤缺陷当量孔径的计算[J]. 无损检测, 2011, 0(9): 68-71
作者姓名:杨晓东  周鹏  杨芳  尚建丽  王杨俊
作者单位:西安建筑科技大学材料科学与工程学院;陕建十一公司;西安交通大学外国语学院;陕西省纺织科学研究所;
基金项目:陕西省教育厅自然科学专项基金资助项目(09JK558)
摘    要:通过理论分析和测试对比,确定钢结构熔透对接焊缝中横孔状焊接缺陷当量孔径适用的对比反射体为:RB,CSK—IC系列试块上φ3mm长横孔及CSK—ⅢA试块上的φ1mm短横孔。试验测出RB,CSK-IC系列,CSK—ⅢA试块与测试用试件表面能耗损失为4dB,将RB,CSK—ⅠC系列试块不同深度φ3mm长横孔和CSK—ⅡA试块上的φ1mm短横孔反射回波幅值分别下调4dB制作DAC(距离-波幅)曲线。经超声波横孔理论回波声压分析,推导出钢结构熔透焊缝中类似于长横孔、短横孔状缺陷当量孔径的计算公式。对于竖孔状缺陷,制作不同孔径、不同厚度钢板的竖通孔反射体,建立波幅-孔径曲线及回归函数,中厚板用一、二次波探伤,薄板用三次波探伤,插入法计算当量孔径,并对这种缺陷当量计算方法进行了验证。

关 键 词:钢结构熔透焊缝  缺陷当量  超声波检测

Caculation of Defects Equivalent Aperture in Utrasonic Testing of Steel Structure Weld
YANG Xiao-Dong,ZHOU Peng,YANG Fang,SHANG Jian-Li,WANG Yang-Jun. Caculation of Defects Equivalent Aperture in Utrasonic Testing of Steel Structure Weld[J]. Nondestructive Testing, 2011, 0(9): 68-71
Authors:YANG Xiao-Dong  ZHOU Peng  YANG Fang  SHANG Jian-Li  WANG Yang-Jun
Affiliation:YANG Xiao-Dong~1,ZHOU Peng~2,YANG Fang~3,SHANG Jian-Li~1,WANG Yang-Jun~1 (1.Department of Material Science and Engineering,Xi'an University of Architecture and Technology,Xi'an 710055,China,2.Shaanxi the Eleventh Construction Engineering Company,Xi'an 712100,3.School of Foreign Languages and Xi'an Jiaotong University,Xi'an 710049,4.Shaanxi Textie Science & Research Institute,Xi'an 710038,China)
Abstract:The paper,through theoretical analysis and test comparison that the applicable contrastive reflectors in calculating the cross bore weld defect equivalent aperture in steel structure weld penetration were the followings, such as RB,φ3 mm long cross bore in CSK-ⅠC series test block andφ1 mm short cross bore in CSK-ⅢA test block.It was revealed in our experiment that the surface energy consumption of RB,CSK-ⅠC series test block, CSK-ⅢA test block and the check bar for test was 4 dB and the DAC curve was made when the dB values of RB,φ3 mm long cross bore in the CSK-ⅠC series test block with various depth as well as the reversed echo ofφ1 mm short cross bore in CSK-ⅢA test block were reduced by 4 dB respectively.By echo sound pressure analysis of Ultrasonic Cross Bore Theory,the formula for calculating the defect equivalent aperture of long and short cross bore in steel structure weld penetration was derived.As to the erect bore defect,the dB-φcurve and regression function were made for making erect through-hole reflector with steel plate of various aperture and thickness.The fault detection was made with primary and secondary wave for medium plate and with tertiary wave for thin plate.The method of Sorting by Insertion,the defect equivalent calculating method,was applied in calculating the equivalent aperture and was tested.
Keywords:Steel structure weld penetration  Defect equivalent  Ultrasonic testing  